3/32" tungsten, about 70 on amperage with the argon at 18... Put more heat on the bung (it's a fillet weld really) than the d.p... ANY competent TIG welder should be able to do this without even thinking about it. Hell, a MIG with stainless wire would be simple too...But not as attractive.